Nothing breaks at its "ideal" strength. Real parts fail from tiny flaws — a scratch, a sharp corner, a microscopic crack — because those flaws concentrate stress at their tips. And a load far too small to break something in one go can still kill it if applied over and over: that's fatigue, where a crack creeps forward a hair per cycle until the part suddenly snaps. Scroll through to see how cracks crowd stress, grow, and finally let go.
Pull on a bar and the stress is spread evenly… until there's a flaw. Lines of force can't pass through a crack, so they crowd around its tip, piling up to many times the average stress. For an elliptical flaw the multiplier is Kt = 1 + 2√(a / r) — longer crack a or sharper tip (smaller radius r) means a bigger spike. That's why brittle things fail far below their ideal strength, why cracks love sharp inside corners, and why a starter notch lets you snap glass or tear a bag. Drag the sliders and watch the lines bunch up.
Apply a load well below the breaking stress, then take it off, again and again. Each cycle a crack at a flaw advances a tiny amount (faster as it lengthens — da/dN ∝ stress²·√a), leaving curved beach marks behind. The part looks fine for thousands of cycles — then the remaining cross-section can no longer hold the load and it fails suddenly, with no warning. Pick a stress level and watch the crack march across; on the right is the S–N curve (stress vs. cycles-to-failure): lower load, exponentially more cycles, until some metals reach a fatigue limit they can survive forever.
The atomic bonds in a solid could in theory hold enormous stress. In practice everything is riddled with microscopic flaws — pores, inclusions, scratches, grain boundaries. Because a flaw concentrates stress at its tip, the material reaches its local failure stress there long before the average stress is anywhere near ideal. Brittle materials (glass, ceramics, cast iron) have nothing to relieve the spike, so they fail from astonishingly small flaws.
Kt = 1 + 2√(a/r) says it all: a long crack with a needle-sharp tip multiplies stress the most. A perfectly round hole only triples it (Kt = 3); a sharp internal corner can multiply it tenfold. The fix is geometry: round the corners, add generous fillets, polish out scratches, and stop-drill a crack — drilling a round hole at the tip blunts it and slashes the concentration.
Under a repeated (cyclic) load, a crack grows a little each cycle even though the peak load is far below the static breaking strength. The growth rate climbs as the crack lengthens (Paris law, da/dN = C·ΔKm), so the last stretch is fast — then the intact area can no longer carry the load and the part fractures suddenly. The broken face shows the story: smooth beach marks from slow growth, then a rough zone from the final snap.
Brittle fracture is fast and clean — little deformation, the pieces fit back together. Ductile fracture stretches and necks down first, absorbing energy and giving warning before it tears. Ductility is forgiving; brittleness is treacherous.
Plotting cyclic stress against cycles-to-failure gives the S–N curve: lower stress buys exponentially more cycles, and many steels show a fatigue limit below which they last indefinitely. Famous lessons: the de Havilland Comet airliners broke up when fatigue cracks grew from the corners of their square windows; Liberty ships cracked clean in two from brittle welds and sharp hatch corners in cold seas. The fixes became standard engineering: round every corner, polish surfaces, keep working stresses under the fatigue limit, and inspect for cracks before they reach the runaway point.